Retraction temperatures tower calibration
An useful Things for calibrating the retraction according to the extrusion temperature.
V.1
01-apr-2018
Must be printed with 0.2mm resolution, no raft.
Temp config: 5 °C every 20 layers from layer 9 to layer 128
Ex for PLA and Cura Gcode file:
- Base: 210°C Layer 0 to layer 9 (0.2mm per layer so 1.6mm)
- Tower:
- Temps by layers :
- Temp #1: 210°C Layer 8 to layer 28
- Temp #2: 205°C Layer 28 to 48
- Temp #3: 200°C Layer 48 to 68
- Temp #4: 195°C Layer 68 to 88
- Temp #5: 190°C Layer 88 to 108
- Temp #6: 185°C Layer 108 to 128 (End)
Remixed From
- Basic Stringing Test by Loohney